doi: 10.17586/2226-1494-2020-20-3-335-345
NONDESTRUCTIVE TESTING OF BALTIC AMBER:OPTICAL ANALYSIS OF MACRO- AND MICROSTRUCTURE
Read the full article
Article in Russian
For citation:
Abstract
For citation:
Verkhovskaia Ia.I., Prokopenko V.T. Nondestructive testing of Baltic amber: optical analysis of macro- and microstructure. Scientific and Technical Journal of Information Technologies, Mechanics and Optics, 2020, vol. 20, no. 3, pp. 335–345 (in Russian). doi: 10.17586/2226-1494-2020-20-3-335-345
Abstract
Subject of Research. We propose a solution to the problem of nondestructive testing formacro- and microstructure of Baltic amber by optical analysis. The considered method provides for high-quality characteristics of materials and amber-made products. Method. The proposed approach was based on the analysis of fluorescence spectra using the “Fluorat-02-Panorama” analyzer. Microstructure study was carried out using Leica DMLM confocal microscope with a resolution less than 1 μm included in Renishaw InVia Reflex laboratory equipment. For macrostructure study, we proposed “Regula” 4305M/MH universal video spectral comparator with “Regula” 100X viewing magnifier. Samples of processed and unprocessed amber from the Palmniken Deposit (Kaliningrad, Russian Federation) with different transparency were studied. Main Results. The fluorescence spectra of Baltic amber with different transparency are presented. It is found that the less transparent samples are characterized by lower fluorescence intensity. We make it clear that the fluorescence spectra of transparent amber with transparency up to 75 % have the form of a wide cascade band with three peaks at the peak of intensity in the range of 650–800 nm. It is noted that the qualitative color characteristics of amber fluorescence have an additive character. It is shown that the destruction of amber can reveal internal and external defects, establish the degree of transparency and distribution of opaque areas in the source material and products made of it. Practical Relevance. The proposed method may be of interest in the field of materials science, research related to identification processes, processing of manufacturing amber-made products. The performed research can be used in the synthesis of high-molecular compounds, in the study of a wide class of organic materials and in the design of organic light emitting diodes.
Keywords: fluorescence spectra, amber, nondestructive testing
Acknowledgements. The authors are grateful to Professor L.T. Zhukova, Director of the Institute of Decorative and Applied Arts and Professor A.I. Potapov, D.Sc., Head of the Instrument Engineering Chair of Mining University for their contribution and comprehensive support in the preparation and carrying out of this study.
References
Acknowledgements. The authors are grateful to Professor L.T. Zhukova, Director of the Institute of Decorative and Applied Arts and Professor A.I. Potapov, D.Sc., Head of the Instrument Engineering Chair of Mining University for their contribution and comprehensive support in the preparation and carrying out of this study.
References
-
Savkevich S.S. Amber. Leningrad, Nedra Publ., 1970, 192 p. (in Russian)
-
Orlov N.A., Uspenskii V.A. Mineralogy of Caustobioliths. Moscow, Leningrad, AS USSR Publ., 1936, 198 p. (in Russian)
-
Anderson K.B. The nature and fate of natural resins in the geosphere–VII. A radiocarbon (14C) age scale for description of immature natural resins: an invitation to scientific debate. Organic Geochemistry, 1996, vol. 25, no. 3-4, pp. 251–253. doi: 10.1016/S0146-6380(96)00137-4
-
Amber, Resinite, and Fossil Resins. Ed. by K.B. Anderson, J.C. Crelling. Washington, American Chemical Society, 1995, pp. 170–192, ACS Symposium Series, vol. 617. doi: 10.1021/bk-1995-0617.fw001
-
Stout E.C., Beck C.W., Anderson K.B. Identification of rumanite (Romanian amber) as thermally altered succinite (Baltic amber). Physics and Chemistry of Minerals, 2000, vol. 27, no. 9, pp. 665–678. doi: 10.1007/s002690000111
-
Amber. Geological Dictionary. 2 volumes. Ed. by K.N.Paffengol'ts et al. Moscow, Nedra Publ., 1978. (in Russian)
-
Barletta E., Wandelt K. High resolution UHV-AFM surface analysis on polymeric materials: Baltic Amber. Journal of Non-Crystalline Solids, 2011, vol. 357, no. 5, pp. 1473–1478. doi: 10.1016/j.jnoncrysol.2010.12.039
-
Chugunov K.V., Parzinger H., Nagler A. An elite burial of the period of early nomads in Tyva. Archaeology, Ethnology and Anthropology of Eurasia, 2002, vol. 10, no. 2, pp. 115.
-
Shedrinskya A.M., Wamplerb T.P., Chugunov K.V. The examination of amber beads from the collection of the state hermitage museum found in Arzhan-2 burial memorial site. Journal of Analytical and Applied Pyrolysis, 2004, vol. 71, no. 1, pp. 69–81. doi: 10.1016/S0165-2370(03)00099-8
-
Beck C.W. Spectroscopic investigations of amber. Applied Spectroscopy Reviews, 1986, vol. 22, no. 1, pp. 57–110. doi: 10.1080/05704928608060438
-
Shi G., Grimaldi D.A., Harlow G.E., Wang J., Wang J., Yang M., Lei W., Li Q., Li X. Age constraint on Burmese amber based on U–Pb dating of zircons. Cretaceous Research, 2012, vol. 37, pp. 155–163. doi: 10.1016/j.cretres.2012.03.014
-
Liu Y., Shi G., Wang S. Color phenomena of blue amber. Gems and Gemology, 2014, vol. 50, no. 2, pp. 134–140. doi: 10.5741/GEMS.50.2.134
-
Bechtel A., Chekryzhov I.Y., Nechaev V. P., Kononov V.V. Hydrocarbon composition of Russian amber from the Voznovo lignite deposit and Sakhalin Island. International Journal of Coal Geology, 2016, vol. 167, pp. 176–183. doi: 10.1016/j.coal.2016.10.005
-
Mills J.S., White R., Gough L.J. The chemical composition of Baltic amber. Chemical Geology, 1984, vol. 47, no. 1-2, pp. 15–39. doi: 10.1016/0009-2541(84)90097-4
-
Galanin M.D. Luminescence of Molecules and Crystals. Moscow, Lebedev Physical Institute, 1999. (in Russian)
-
Levshin L.V., Saletckii A.M. Luminescence and its Measuring Methods. Molecular Luminescence. Moscow, MSU, 1989, 277 p. (in Russian)
-
Parker C.A. Photoluminescence of Solutions. Elsevier Publishing Company, 1968, 544 p.
-
Gorobets B.S., Rogojine A.A. Luminescent Spectra of Minerals. Reference-book. Moscow, 2002, 302 p.
-
Anderson K.B., Winans R.E., Botto R.E. The nature and fate of natural resins in the geosphere-II. Identification, classification and nomenclature of resinites. Organic Geochemistry, 1992, vol. 18, no. 6, pp. 829–841. doi: 10.1016/0146-6380(92)90051-X
-
Grimaldi D.A. Amber: Window to the Past. New York, Harry N. Abrams, 2003, 216 p.
-
Matuszewska A., Czaja M. Aromatic compounds in molecular phase of Baltic amber-synchronous luminescence analysis. Talanta, 2002, vol. 56, no. 6, pp. 1049–1059. doi: 10.1016/S0039-9140(01)00610-5
-
Wert C.A., Weller M., Schlee D., Ledbetter H. The macromolecular character of amber. Journal of Applied Physics, 1989, vol. 65, no. 6, pp. 2493–2499. doi: 10.1063/1.342795
-
Alekseeva A.V., Samarina L.A. The question of the chemical structure of amber. Chemistry of Natural Compounds, 1966, vol. 2, no. 6, pp. 351–356. doi: 10.1007/BF00564222
-
Kariakin A.V., Gribovskaia I.F. Optical Spectroscopy and Luminescence Methods in Analysis of Natural and Waste Waters. Moscow, Chemistry Publ., 1987, 304 p. (in Russian)