The effect of SiO2/Si system irradiation by pulsed ytterbium fiber laser PLI-1-50 on the morphology and system structural properties has been investigated. It is shown that during surface irradiation of the monocrystalline silicon wafer covered by a thin layer of thermally grown silicon dioxide (SiO2), there are significant structural changes associated with localization of the silicon strips of slip-lines and grid of slip-lines on the surface formed by the intersection of these strips. Phonon theory of the resulting microstructural topography has been considered.


Keywords: laser irradiation, dislocations, slip-lines, grid of slip-lines, mechanical stresses, plastic deformation, recrystallization, nanocomposite

Creative Commons License

This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License
Copyright 2001-2026 ©
Scientific and Technical Journal
of Information Technologies, Mechanics and Optics.

Яндекс.Метрика